Study on natural ignition characteristic test of No. 13 coal seam
Li Guohui1, Bi Jianyi1, Zhang Hui2, Sun Liang3
1. Xiegou Mine, Shanxi Xishan Jinxing Energy Corporation Ltd., Lvliang 033602, China; 2. School of Safety Science and Engineering, Liaoning Project Technology University, Fuxin 123000, China; 3. Shenyang Institute of Coal Group cor. Ltd., Fushun 113122, China
In order to prevent No. 13 coal seam spontaneous combustion in Xiegou Mine, spontaneous ignition test simulating spontaneous combustion of the coal seam, temperature variation rule was studied by analyzing 23107 working face coal sample, parameters like minimum natural ignition period, critical temperature, dry crack temperature and active temperature were settled, the test result showed that coal sample temperature rising fastened its oxidation rate, when coal sample temperature lowered than stagnation temperature, the oxidation rate got slow, when coal sample temperature larger than stagnation temperature, the oxidation rate got fast, when coal sample temperature larger than dryness temperature, oxidation rate increases significantly. The temperature of gas marker in the coal spontaneous combustion was used to predict the degree of coal spontaneous ignition, providing reference for fire prevention and control in Xiegou Mine.
李国辉1,毕建乙1,张 辉2,孙 亮3. 斜沟煤矿13号煤层自然发火特性试验研究[J]. 煤炭与化工, 2018, 41(4): 111-115.
Li Guohui1, Bi Jianyi1, Zhang Hui2, Sun Liang3. Study on natural ignition characteristic test of No. 13 coal seam. CCI, 2018, 41(4): 111-115.