| Analysis and treatment of wax formation in methanol synthesis |
| Tang Jian, Sui Xingbing, He Ying, Tao Yunliang |
| Methanol Department, Zhongtianhechuang Energy Corporation Ltd., Erdos 017000, China |
|
|
|
|
Abstract In the production of low temperature coal to methanol by copper catalysis, the formed paraffin can easily lead to the blockage of the final cooler and separator, thus influencing the production of methanol. The reasons of paraffin formation in methanol synthesis and the prevention and treatment measures were discussed. It is put forward by controlling the water vapor in the feed gas and the reaction temperature in the range of 210 ~ 260 ℃, reducing the loop pressure in synthesis system and improving airspeed, the paraffin precipitation can be reduced. And Low pressure steam is used to heat the final cooler to removetheparaffin precipitation.
|
|
|
|
|
|
| [ 1 ] 黄金钱,刘金辉,仇 冬. 合成甲醇过程中结蜡的原因及预防处理措施[J].化学工业与工程技术,2006,27( 2 ):44 - 46.
[ 2 ] 杨凤英,梁 慧,蔡德会,等. 浅谈甲醇在线煮蜡与传统煮
蜡[ J ]. 氮肥技术,2007,28( 6 ):38,39.
[ 3 ] 丁慧平,穆晨霞. 甲醇合成结蜡的原因及处理[ J ]. 广东化
工,2005( 11 ):68,76.
[ 4 ] 杨玉兰,刘振洪,左继功,等. 甲醇合成催化剂使用经验总结[ J ]. 天然气化工,2000,25( 2 ):37 - 43.
[ 5 ] 杨林君. 甲醇生产过程中结蜡的预防及处理[ J ]. 化工文摘,2008( 2 ):6I-62. |
|
|
|